Unlike other targets on the market, the LUXOR gold/palladium-targets comes pre-mounted on a convenient push-fit holder. Simply push the target into place, there’s no need to handle and replace fragile disks or use screwdrivers or other special tools.
€1,235.00 €1,469.65

Product Details

Description

  • Pre-mounted targets: screwdrivers or other special tools are not required for changing targets, no more delicate handling of thin metal discs
  • Perfect electrode contact
  • Longer target lifetime: the combination of low voltage and coating current together with the positioning of the magnetic field ensures that the lifetime of a LUXOR target is longer. About 1000 (for 10nm film thickness) to 5000 (for 2nm film thickness) coating cycles are possible per target, depending on the required coating thickness. Gold is typically coated with a layer thickness of 5 to 15 nm, while for platinum, layer thicknesses of 2 to 5 nm are applied.
  • Cheaper: the positioning, dimensions and construction of the various components in the plasma reactor of a LUXOR coater are optimized such that usually encountered “race tracking” (uneven erosion of a target) is reduced to a minimum
  • Quick: The time for coating a 10 nm gold layer is typically 2 min and 1.5 min for a platinum layer of 5 nm. The entire coating process with the preliminary vacuum creation and return to atmospheric pressure after the process takes about 5 to 6 min.
  • For use in air or argon

More Information

More Information
Diameter Ø30mm
Thickness 0,1mm
Purity 80% (Gold) / 20% (Palladium)